Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Will flash rusting or brown spots occur on Wearlon coated cold rolled steel?

0
Posted

Will flash rusting or brown spots occur on Wearlon coated cold rolled steel?

0

If sandblasted, cold rolled steel when left in storage for any period of time, a flash-rust additive should be applied before coating. The preferred flash-rust additive, Flash Shield Rust Inhibitor 104-K, can be supplied by Plastic Maritime or purchased from UltraChem LLC (phone 713-641-4245). If purchased from UltraChem, it should be cut 30:1 with water. It will delay flash rusting for 3 to 5 days. It is specifically formulated so that Wearlon coatings can be applied directly over it without loss of adhesion. Pre-heating of sandblasted steel to approximately 120° – 140° F.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123