Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Why is the 18 yellow “D” casting crumbling or brittle?

0
Posted

Why is the 18 yellow “D” casting crumbling or brittle?

0

• “D” or Deox alloys usually will have silicon in them to help casters reduce oxidation and porosity. However, these deoxidizers will generally increase the metals temper, making them slightly harder. If the metal is over-heated, this will make metal harder to the point of brittleness. Remember Hoover does custom casting and specializes in unusual colors and metals.