Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Why is CO-NETIC AA alloy offered in both Perfection Annealed and Stress Annealed types?

0
Posted

Why is CO-NETIC AA alloy offered in both Perfection Annealed and Stress Annealed types?

0

CO-NETIC AA alloy always requires a special annealing process to develop its full magnetic properties. If fabrication involves severe drawing, forming or welding operations, the properties of the alloy will be adversely affected, and annealing must be done after the manufacturing operations are complete. For such applications, CO-NETIC AA alloy Stress Annealed is offered. It has better formability characteristics and costs less. If the application does not involve severe drawing, forming or welding, then CO-NETIC AA alloy Perfection Annealed may be used, and the final annealing step may be avoided. This is because CO-NETIC AA alloy Perfection Annealed has been fully annealed before shipment and is ready to perform as a magnetic shield. CO-NETIC AA alloy Perfection Annealed has a large, open grain structure and must not be used when the shield fabrication involves severe drawing, forming or welding.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123