Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Why are air-entraining admixtures now being used in Controlled Low Strength Material (CLSM)?

0
Posted

Why are air-entraining admixtures now being used in Controlled Low Strength Material (CLSM)?

0

The inclusion of 15-35% entrained air in CLSM improves flowability, minimizes segregation and settlement, lowers unit weight (90-110 pcf), and controls ultimate strength development. In addition, air, gas and water permeability properties will improve as CLSM air contents increase.