Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What is the welding procedure for the weld-on products?

0
Posted

What is the welding procedure for the weld-on products?

0

• Align and tack the wear point to the other piece before heating. • Preheat the area to be welded to approximately 300F. • Weld using MIG wire welder or #7018 low hydrogen arc welding rod or stainless steel welding rod. • Allow pieces to cool slowly by placing them in some type of insulation.