Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What is the safe limit for ammonia in contact with brass to prevent stress corrosion cracking?

0
Posted

What is the safe limit for ammonia in contact with brass to prevent stress corrosion cracking?

0

A There is no acceptable limit – it is essential that internal stresses are removed as far as possible by a stress relief anneal at 250-350oC for 1/2 to 1 hour.