Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What is the recommended minimum bend radius for Corning Specialty fiber?

0
10 Posted

What is the recommended minimum bend radius for Corning Specialty fiber?

0
10

Bend radius impact on optical performance is highly dependent upon the specific application, so Corning is unable to recommend specific guidelines for customer use. In general, Corning recommends a minimum bend radius of 25mm for standard fiber, however some specialty fibers may withstand a smaller bend radius.