Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What is being done to mitigate tin whisker growth?

growth mitigate tin whisker
0
Posted

What is being done to mitigate tin whisker growth?

0

We have chosen matte tin as the lead finish for all lead-free products. The package is annealed within 24 hours at 150°C for 1 hour after lead plating. This is the industry-accepted method for mitigating tin whisker growth.