Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What are the thicknesses of DuPont interlayers?

0
Posted

What are the thicknesses of DuPont interlayers?

0

DuPont™ SentryGlas® ionoplast interlayers start at 0.035 in. (0.90 mm) for general safety glass and hurricane-rated glass; 0.060 in. (1.56 mm) for architectural glazing such as canopies, railings and facades; and up to .090 in. (2.28 mm) and above for large missile impact an high security bomb blast systems. The typical thicknesses of Butacite® PVB are 0.030 in. (0.78 mm) for general-purpose safety glazing, .060 in. (1.56 mm) for burglar resistance, bomb blast resistance, and overhead glazing laminates made with heat-treated glasses; and .090 in. (2.28 mm) for hurricane-rated systems.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.