Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What are the sample sizes required for DSS testing?

DSS sample Testing
0
Posted

What are the sample sizes required for DSS testing?

0

The following are the samples sizes required for various testing on a DSS material. – Pitting Test: 25mm X t X 50 mm where t (thickness) should be 10 mm. If the material has more thickness then you should cut the sample to 10mm in thickness. – Crevice Test: 25mm X t X 50 mm where t (thickness) should be 10 mm. If the material has more thickness then you should cut the sample to 10mm in thickness. – Chloride Stress Test: 15mm X 15mm X 125mm – Ferrite Test: 1 inch X 1inch – Sulphide Stress Corrosion Test (SSCC): 15mm X 15mm X 150mm – Intergranular Corrosion (IGC): 25mm X t X 25mm (where thickness can be anything) – Hardness Test: 25mm X t X 25mm (where thickness can be anything) – Impact Test: We will need 6 samples from the same material of the size 15mm X 15mm X 55 mm – Tensile Test: 16mm X 16mm X 150mm With respect to Hydrogen Induced Cracking (HIC) testing on a flange, we will need to get a sample of the following size: 20 mm width X 100 mm length X T. Please note that T (thickness)

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123