Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What are the critical pitting and crevice corrosion temperatures for copper nickels in chloride environments?

0
Posted

What are the critical pitting and crevice corrosion temperatures for copper nickels in chloride environments?

0

A Copper nickels do not behave in the same way as stainless steels do towards corrosion by chlorides and these parameters are not appropriate to them. They do not have a critical temperature limit.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123