Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What are some Specific IntegraBase tests and their expectations?

0
Posted

What are some Specific IntegraBase tests and their expectations?

0

Resilient Modulus – Expect a doubling at 40 deg. C at a lower rate of loading – tripling is not out of the question. Marshall Stability – Typically a 25-30% increase Indirect tensile Strength – Tensile strength at higher temps usually doubles Wheel Tracking – 40 Deg C, half of the depth of the track of the control Stripping – We are always better with wet strength. IntegraBase tends to lose a higher percentage after soaking (retained strength ratio), but looking at it relatively, IntegraBase still has a higher wet strength both before and after soaking when compared with an unmodified sample.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123