What are some characteristics of a poorly installed clear bra?
The idea is to basically install a one dimensional piece of film on a 3 dimensional object. This creates plenty of issues for all but the most competent installers: • Stretch marks- Visually significant change in texture due to improper stretch technique. A small amount is acceptable around compound curves but should be very minimal. • Silvering- Tiny white or silver looking specs clumped together caused by adhesive disturbance where the film had adhered unevenly to the body panel due to improper technique. • Misalignment- Excessive gap from body edge to film end caused from improper alignment and stretching or poor pattern design. 1/16 gap is the target. • Air/ water bubbles- Poor squeegee technique has left either air or water where it shouldn’t be. • Lift marks- A straight line raised slightly represents where the film was improperly pulled back up after adhering thus disturbing the adhesive at the point it was pulled back to. • Dust or Hair- Dirty installation environment leaving u