Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Im using Outershield® 71M (E71T-1) flux-cored wire with 75Ar/25CO2. Why am I getting gas marks on the weld surface?

flux-cored Gas marks wire
0
Posted

Im using Outershield® 71M (E71T-1) flux-cored wire with 75Ar/25CO2. Why am I getting gas marks on the weld surface?

0

The fast freezing rutile slag on an E71T-1 Outershield® wire gives it excellent out-of-position characteristics, but can also trap gases under the slag as the weld solidifies, resulting in gas marks. Gas marks are more commonly observed welding at high procedures under a high Argon blend shielding gas.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123