I am trying to find out if there is any research or literature regarding the drying shrinkage of shotcrete. Can you help?
See ACI 506R, Sec. 1.7 (ACI document). Typical shrinkage varies in the range of 0.06 to 0.10 percent after 28 days drying. It is typically slightly higher than similar strength concrete, mostly due to less and/or smaller coarse aggregate in the shotcrete mix. (back to top) Question 44: I’ve been a pool builder all my life and I use your magazine as a technical source and I really enjoy it. I found a conflict: In Shotcrete Summer 2004, page 30, the answer to the second question suggests the use of 8% as batched air content with max sized coarse aggregate of 3/8 inch. The conflict I have is that a) won’t 8% as batched drop to 1-2% after wet gunning? and b) previous articles suggested the use of 15-22% air as batched to help get it through the hose and to achieve 8% in place. Can you clarify? Answer: For over 30 years in Canada we have been designing wet mix shotcrete for exterior exposure (rock-slope stabilization, tunnel portals, canals and beams, infrastructure rehabilitation, etc.) to