How do I make Ionic/Colloidal Silver using the heat method?
Bring 2 cups of distilled water to the boil in a nonmetal container. Pour into a glass jar and immerse about 75% of the silver wires. Let the unit run for 15 to 20 minutes for 5-8 PPM . The water is brought to the boil simply to give a standard for heat. Heating is necessary to increase the conductivity of the water.