Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

How are the Ag nanotriangles released from the glass substrate into solution after they have been fabricated by NSL?

0
Posted

How are the Ag nanotriangles released from the glass substrate into solution after they have been fabricated by NSL?

0

The Ag nanotriangles are firstly made by NSL on glass slide, then incubated in 1 mM hexandecanethiol (other alkanethiol works as well) for 49-96 h. After incubation, rinse the samples thoroughly with neat ethonal. Lastly, sonicate the samples in ethanol for 3-5 min and you can observe the color on the glass slide is gone.

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123