Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Do I need to post heat the Wearlon coated surface?

Coated heat wearlon
0
Posted

Do I need to post heat the Wearlon coated surface?

0

All Wearlon coatings will cure on substrates that are coated at surface temperatures above 40°F or at room temperature. These coatings are excellent performers and can be put into service the next day or preferably a week later to allow further curing at room temperature. If desired post heating the next day after coating will result in higher cross-linked density and therefore will have better abrasion properties. Some Wearlon coated substrates are post heated at temperatures as high as 300°F for 30 minutes before being put into service.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123