Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Can Maxims standard reflow temperature range lead-free and leaded parts be mixed during board reflow? What reflow temperature would be used in this scenario?

0
Posted

Can Maxims standard reflow temperature range lead-free and leaded parts be mixed during board reflow? What reflow temperature would be used in this scenario?

0

Maxim’s lead-free termination parts can be mixed with leaded termination parts and reflowed at a lower temperature (240°C) with proper reflow conditions and compatible solder paste. However, the reliability of Maxim parts with leaded terminations are not guaranteed at higher reflow temperature (above 240°C). Some reference sources show data that define a reduction in solder joint reliability by as much as 33% less than Eutectic solder joints when lead and lead-free metallurgies are mixed.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.

Experts123