Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Are nickel-base alloys subject to stress corrosion cracking?

0
Posted

Are nickel-base alloys subject to stress corrosion cracking?

0

A. As far as chloride stress corrosion cracking (SCC) is concerned, the high nickel contents of these materials make them immune to this particular form of stress corrosion. However, the nickel base alloys are sensitive to other forms of environmental stress corrosion cracking.