Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Are 90-10 and 70-30 copper nickels susceptible to stress corrosion cracking?

0
Posted

Are 90-10 and 70-30 copper nickels susceptible to stress corrosion cracking?

0

A They do not experience chloride or sulphide stress corrosion. They have a high resistance to ammonia stress corrosion compared to other copper alloys and do not require a stress relief anneal for seawater service.