Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Any special care required in formability and welding?

formability special welding
0
Posted

Any special care required in formability and welding?

0

The equipments used for 304 can also be used for 201 including the lubricating however we advice the following guidelines to be followed: Deep drawing ratio: 2 Elongation by spinning : 30% Production sequence in one go All welding equipments same as 304 Grade can be used.